1. Utilize skilled welders with rejection rate of less than five (5) percent on a joint basis or 0.2% ona linear basis in the most recent past 12 months. 2. Use approved Welding Procedure Specification (WPS). 3. Visually inspect the root and cap pass during the welding process with a JV inspector. 4. Perform 100% of radiographic testing (RT) or advanced ultrasonic testing (UT) for circumferential, longitudinal, Spiral groove welds 5. RT and advanced UT to be interpreted by ASNT Level Ill personnel. 6. For all welds were the point 4 & 5 is not applicable test will be performed by Liquid Penetrant Method (Bubble Test or Soap test) 7 . Flexibility Analysis will be performed only in case the weld is located in elbow 8. All welds shail be tested by Dye Liquid Penetrant on the root pass and cap pass of the welds.