Está en la página 1de 4

PT SHIMANO BATAM DOC. NO.

: PPSF - A - 31
REVISION : A
WORK INSTRUCTION EFFECTIVE DATE : 6-Dec-17
SHEET : 1 of 4
TITLE : Procedur Operation Spectroquant PREPARED BY : Edwin Otniel L Toruan
For Chromium (VI) APPROVED BY : CHAI MIN CHONG

1 2

1. Take sample solution from TK20 ,then 2. Open top component spectroquant and it
check pH, allowed pH range (1-9). If pH <1 then conditions automatically check
add sodium hydroxide. If pH >9 then add sulfuric
acid. 2. Buka bagian atas spectroquant dan
spectroquant mengecek kondisinya secara
1. Ambil larutan sampel dari TK20 lalu cek pH, otomatis.
kisaran pH yang diperbolehkan (1-9). Jika pH <1
maka tambahkan sodium hidroksida, jika pH >9
maka tambahkan asam sulfat.
PT SHIMANO BATAM DOC. NO. : PPSF - A - 31
REVISION : A
WORK INSTRUCTION EFFECTIVE DATE : 6-Dec-17
SHEET : 2 of 4
TITLE : Procedur Operation Spectroquant PREPARED BY : Edwin Otniel L Toruan
For Chromium (VI) APPROVED BY : CHAI MIN CHONG

3.1

3.1 Press button " " then appear setup menu ,and choose zero callibration by pressing " ".

3.1 Tekan tombol " " lalu muncul menu pengaturan, dan pilih penyesuaian di nol dengan menekan
tombol " ".

3.2

3.2 Take zero cell, then put and press down it to spectroquant. Spectroquant will be automatically zero
callibrating.

3.2 Ambil zero cell, lalu letakkan dan tekan zero cell ke dalam spectroquant. Spectroquant akan
otomatis menyesuaikan ke nol
PT SHIMANO BATAM DOC. NO. : PPSF - A - 31
REVISION : A
WORK INSTRUCTION EFFECTIVE DATE : 6-Dec-17
SHEET : 3 of 4
TITLE : Procedur Operation Spectroquant PREPARED BY : Edwin Otniel L Toruan
For Chromium (VI) APPROVED BY : CHAI MIN CHONG

4 5

4. Take Cr auto selector barcode and put 5. Take cell and take a little powder reagen Cr
it to spectroquant. -1 .
4. Ambil Cr auto selector barcode dan 5. Ambil dan ambil sedikit bubuk reagen Cr - 1.
masukkan kedalam spectroquant.

6 7

6. Put powder reagen Cr - 1 to cell and add 6 7. Shake cell hard to dissolve powder reagen
drop off reagen Cr - 2 Cr - 1
7. Guncangkan cell dengan keras untuk
6. Masukkan bubuk reagen Cr - 1 kedalam cell melarutkan bubuk reagen Cr - 1.
dan tambahkan 6 tetes reagen Cr - 2.

8 9

8. Add 5 ml sample to cell, mix it. 9. Shake cell again and wait 1 minute
because reagen need time to react with
8. Tambahakan 5 ml sample kedalam sample.
cell, campurkan.
9. Guncangkan lagi cell dan tunggu 1
menit karena reagen membutuhkan waktu
untuk bereaksi dengan sampel.
PT SHIMANO BATAM DOC. NO. : PPSF - A - 31
REVISION : A

WORK INSTRUCTION EFFECTIVE DATE : 6-Dec-17


SHEET : 4 of 4
TITLE : Procedur Operation Spectroquant PREPARED BY : Edwin Otniel L Toruan
For Chromium (VI) APPROVED BY : CHAI MIN CHONG

10 11

10. Move solution to cuvet cell . 11. Put cell to spectroquant.

10. Pindahkan larutan kedalam kuvet cell. 11. Masukkan cell kedalam
spectroquant.

12 13

12. Concentration of the solution 13. Lift Cr auto selector and cuvet
automatically check. cell, then close top component
spectroquant. It automatically turn
12. Konsentrasi dari larutan akan di cek off.
secara otomatis . Dont forget to wash cuvet cell and cell
immidiately.

13. Angkat Cr auto selector barcode


dan kuvet cell, lalu tutup bagian atas
spectroquant. Spectroquant akan
otomatis mati. Jangan lupa untuk
segera mencuci kuvet cell dan cell .